Differential Scanning Calorimeter

Thermal transition measurement for polymers, metals, and pharmaceuticals

PRODUCT OVERVIEW

A differential scanning calorimeter for measurement of thermal transitions including melting, crystallisation, glass transition, and reaction enthalpies. Essential for polymer characterisation, pharmaceutical analysis, and materials research.

TECHNICAL SPECIFICATIONS

Temperature Range-90°C to 700°C
Heating Rate0.01 to 200°C/min
Sensitivity<0.2µW
AtmosphereN₂, Ar, air, O₂
Sample Mass1 to 100mg
CalibrationMulti-point temperature and enthalpy

APPLICATIONS

  • Polymer melting and crystallisation
  • Glass transition temperature
  • Oxidation stability
  • Pharmaceutical purity
  • Reaction kinetics

KEY FEATURES

  • High sensitivity for small thermal events
  • Wide temperature range
  • Multiple atmosphere capability
  • Comprehensive thermal analysis software

REQUEST A QUOTATION

Contact our technical team for pricing, availability, and technical consultation on this product.

Request a Quotation

Category

Thermal Analysis Equipment

Back to Material Characterisation Equipment